Thread Rating:
  • 0 Vote(s) - 0 Average
  • 1
  • 2
  • 3
  • 4
  • 5
Recovered 2-diameter PPB.
03-13-2020, 12:32 PM,
#25
RE: Recovered 2-diameter PPB.
Jim,
That sounds almost exactly the alloy what Kurt is using .
Do I recall correctly that the 95-5 is 95tin/5Antimony?

Interestingly, I ran across a copy I made of a report by Dan Theodore on antimony containing alloys he
found to be working /shooting well with long ogive bullet designs. His final recommendation was
97% lead, 1.5% Antimony, 1.5% tin.
My 9+1 COWW/Lino alloy is estimated to be:
94.5% lead/4.5%Antimony/1%tin. Lee hardness 15.4
Arnie
Reply


Messages In This Thread
Recovered 2-diameter PPB. - by Distant Thunder - 03-04-2020, 10:11 PM
RE: Recovered 2-diameter PPB. - by Don McDowell - 03-05-2020, 12:47 AM
RE: Recovered 2-diameter PPB. - by Kurt - 03-05-2020, 11:15 AM
RE: Recovered 2-diameter PPB. - by MikeT - 03-05-2020, 12:10 PM
RE: Recovered 2-diameter PPB. - by Randy Bohannon - 03-05-2020, 03:44 PM
RE: Recovered 2-diameter PPB. - by Kurt - 03-05-2020, 04:03 PM
RE: Recovered 2-diameter PPB. - by Don McDowell - 03-05-2020, 08:05 PM
RE: Recovered 2-diameter PPB. - by Kurt - 03-07-2020, 12:16 PM
RE: Recovered 2-diameter PPB. - by J.B. - 03-07-2020, 06:19 PM
RE: Recovered 2-diameter PPB. - by Kurt - 03-07-2020, 06:19 PM
RE: Recovered 2-diameter PPB. - by Kurt - 03-07-2020, 08:15 PM
RE: Recovered 2-diameter PPB. - by J.B. - 03-08-2020, 02:35 AM
RE: Recovered 2-diameter PPB. - by beltfed - 03-12-2020, 10:44 PM
RE: Recovered 2-diameter PPB. - by beltfed - 03-13-2020, 12:32 PM
RE: Recovered 2-diameter PPB. - by Kurt - 03-13-2020, 03:43 PM